The stability of the glass gob plays a pivotal role in the production process of glass bottles, and even plays a decisive role in some cases. Therefore, how to improve the stability of glass bottle feed liquid has become an important topic that many glass factories are concerned about.
In the production of glass bottles, after the raw materials for making glass bottles are heated and melted by a kiln, they are then supplied to the bottle-making machines below with different weights and different types of materials through an automatic cutting feeder to complete the process. The production of glass bottles, and the stability of the glass gob is very important, which can play a pivotal role in production.
In the original glass bottle factory, most of the furnaces were semi-gas furnaces. The temperature of the glass liquid in the feeder basin changed greatly, and the size of the cut glass liquid group was also different. Sometimes only oil guns (steam spray) and The observation hole is slowly adjusted, and it is difficult to use after it is led to the bottle making machine, resulting in a high defective glass bottle, which also affects the development of the glass bottle factory for a period of time.
With the continuous advancement of the urban process, in recent years, the kilns of the glass bottle factory have been changed to full gas, and the feed ports of the feeders have also been replaced with high-temperature electric heating silicon carbide rods installed in the feed basin according to a certain proportion. Electric heating to adjust the temperature, electric heating can control the temperature change in the material basin within 5–10 degrees up and down, the gobs supplied to the bottle making machine are uniform and the elasticity is also very good, thus completely solving the problem of glass The stability of the liquid, so that the material liquid is very easy to use in the production of the bottle making machine, and the production rate of the bottle is also greatly improved.
Post time: May-25-2022